Scarify the road base. |
 |
Break the large lumps using a disc. |
 |
Apply the water / CBR PLUS mixture. |
 |
Mix the layer, using a grader to achieve an even moisture content, throughout the mixed layer. |
 |
Add more water, without product, if required toraise the moisture content to OMC +1%. |
 |
Compact, using a pad-foot compactor. |
 |
Compact in layers. |
 |
Final shape and compacting, using a pad-foot and smooth-drum roller. |
 |
Final surface rolling, with smooth-drum roller. |
 |
Finished road, open for traffic. |
 |